| Titanium Sheet and Plate | Commercially pure Grades 1–4; Grade 5 Ti-6Al-4V; Grade 23 Ti-6Al-4V ELI | ASTM B265; commonly supplied to relevant aerospace, pressure-vessel, or industrial purchase specifications |
Titanium Sponge and alloying elements are melted into a consolidated ingot, often using vacuum or inert-atmosphere melting. | The ingot is heated and reduced by hot forging and hot rolling; repeated passes improve thickness uniformity and structure. | Solution treatment, annealing, or stress relieving is selected according to grade, thickness, and required mechanical properties. | Cutting, leveling, pickling, chemical milling, or precision machining may be applied. Surface contamination is carefully controlled. | Chemical analysis, dimensions, tensile testing, hardness, surface examination, and ultrasonic testing for specified plate grades or thicknesses. | Heat exchangers, chemical-processing equipment, aircraft structures, marine components, and corrosion-resistant fabrication. | Choose Grade 2 for broad corrosion resistance and formability; choose Grade 5 for higher strength; choose Grade 23 where enhanced fracture toughness and lower interstitial limits are required. |
|
titanium bars and Billets | Grades 2, 5, 9 Ti-3Al-2.5V, and 23 | ASTM B348 for bars and billets; additional dimensional and heat-treatment requirements may apply | A controlled alloy ingot is produced, inspected for chemistry, and cropped to remove segregated or defective ends. | Open-die or closed-die forging, rotary forging, and hot rolling convert the ingot into round, square, or rectangular bar stock. | Annealing or solution treatment and aging may be used. Grade 5 commonly receives heat treatment to develop high strength. | Peeling, centerless grinding, turning, straightening, and chamfering are used to achieve the ordered diameter and surface condition. | Tensile testing, hardness, ultrasonic inspection, dimensional checks, and visual examination are commonly specified. | Fasteners, shafts, landing-gear components, valve parts, medical instruments, and machined structural parts. | Confirm diameter tolerance, straightness, grain-flow requirements, heat-treatment condition, and ultrasonic acceptance level before ordering. |
| Titanium Forgings | Grade 5 Ti-6Al-4V; Grade 23; selected near-alpha and alpha-beta alloys | ASTM B381 for titanium and titanium-alloy forgings; product-specific qualification may also be required | Billet is cut to a calculated charge size and heated in a controlled atmosphere to reduce oxidation and alpha-case formation. | Blocker forging, finish forging, and sometimes isothermal or close-die forging produce the required geometry and directional grain flow. | Post-forging annealing, solution treatment, aging, or stress relief establishes the specified strength and ductility balance. | Flash removal, shot peening where permitted, machining allowances, surface cleaning, and final precision machining are performed. | Dimensional inspection, tensile testing, microstructure evaluation, dye-penetrant testing, and ultrasonic inspection are common. | Aircraft fittings, engine parts, pressure components, orthopedic components, and high-strength mechanical assemblies. | Forgings are preferred when grain flow, fatigue performance, and lower material waste are more important than the lowest initial tooling cost. |
| Titanium Seamless Tube and Pipe | Commercially pure Grades 1–4; Grade 9; Grade 5 for higher-strength service | ASTM B338 for condenser and heat-exchanger tubes; ASTM B861 for seamless pipe and tube | A hollow billet or suitable round billet is prepared with verified chemistry and a clean, defect-free surface. | Piercing, extrusion, hot working, and cold drawing reduce wall thickness and control outside diameter without a longitudinal weld. | Intermediate annealing may be used between drawing passes; final annealing is selected for strength, ductility, and corrosion performance. | Sizing, straightening, cutting, end finishing, pickling, and cleaning produce the required dimensional and surface condition. | Eddy-current or ultrasonic testing, hydrostatic or pneumatic testing where specified, dimensional checks, and tensile testing. | Desalination, chlor-alkali equipment, condensers, chemical-processing systems, and offshore heat-transfer installations. | Specify outside diameter, wall thickness, length, straightness, end condition, test pressure, and whether seamless construction is mandatory. |
| Titanium Welded Tube and Pipe | Grades 2 and 7 for corrosion service; Grade 9 for lightweight structural tubing | ASTM B862 for welded titanium and titanium-alloy pipe; project specifications define weld and testing requirements | Flat strip or sheet is slit to width, cleaned, and formed into a cylindrical shape in a controlled production line. | Longitudinal edges are joined, commonly by gas-tungsten-arc, plasma, or another qualified inert-gas welding process. | Post-weld annealing or sizing may be applied when required to restore ductility, reduce residual stress, or achieve final dimensions. | Bead conditioning, sizing, straightening, pickling, cutting, and end preparation are completed after welding. | Weld-zone visual inspection, radiographic or ultrasonic examination when specified, eddy-current testing, hydrostatic testing, and dimensional checks. | Large-diameter process lines, heat exchangers, seawater systems, chemical plants, and architectural or structural tubing. | Welded products can be economical for larger diameters; confirm weld qualification, inert-gas protection, weld-zone testing, and allowable pressure. |
| Titanium Wire and Welding Filler | Commercially pure Grades 1–2; Grade 5 Ti-6Al-4V; Grade 23 for selected medical and aerospace uses | ASTM B863 for titanium and titanium-alloy wire; welding filler classification may depend on the applicable welding code | Clean rod or bar feedstock is selected for chemistry, surface quality, and compatibility with the intended base metal. | Hot rolling and repeated cold drawing reduce the feedstock to the target wire diameter. | Intermediate vacuum or inert-atmosphere annealing prevents excessive work hardening and maintains ductility during drawing. | Precision sizing, spool winding, straight-cutting, surface cleaning, and controlled packaging protect the wire from contamination. | Chemical analysis, diameter checks, tensile testing, surface inspection, and weldability or lot traceability documentation. | Gas-tungsten-arc welding, aerospace repair, additive manufacturing feedstock, medical devices, and fine wire components. | Match filler chemistry to the base alloy and welding procedure; require clean handling and sealed packaging for critical applications. |
| Titanium Powder for Additive Manufacturing | Grade 5 Ti-6Al-4V and Grade 23 Ti-6Al-4V ELI | ASTM F2924 for Ti-6Al-4V powder used in additive manufacturing; purchaser requirements define powder quality | Alloy feedstock is melted and atomized under vacuum or inert gas to produce spherical powder particles. | The powder is sieved and classified into a controlled particle-size distribution suited to the selected additive process. | Printed parts commonly receive stress relief, hot isostatic pressing, solution treatment, aging, or annealing according to design requirements. | Parts are depowdered, support structures are removed, and machining, blasting, polishing, or chemical finishing may follow. | Powder morphology, particle-size distribution, flowability, apparent density, oxygen and nitrogen content, and printed-part mechanical testing. | Complex aerospace parts, lightweight lattices, dental components, orthopedic implants, and low-volume customized production. | Control oxygen pickup, moisture, reuse cycles, powder traceability, and compatibility with the selected laser or electron-beam process. |
| Titanium Fasteners and Machined Components | Grade 2 for corrosion resistance; Grade 5 for high strength-to-weight performance | Applicable ASTM or ISO product standards depend on the fastener type, thread form, dimensions, and application | Certified bar, wire, or forgings are selected with full heat and material traceability. | Cold heading, hot forging, or CNC turning forms the basic part before threading and secondary operations. | Stress relieving, annealing, or solution treatment and aging are selected according to alloy and required mechanical properties. | Thread rolling or cutting, deburring, surface cleaning, passivation where specified, and dimensional calibration complete the component. | Thread gauges, dimensional inspection, tensile or proof-load testing, hardness, surface inspection, and lot traceability review. | Marine assemblies, chemical equipment, aircraft structures, bicycles, sporting equipment, and medical or laboratory hardware. | Specify thread standard, strength class, preload requirements, galling-control method, surface condition, and compatibility with mating materials. |