| 1. Grade Selection |
| Commercially Pure Titanium Grade 1 | Unalloyed titanium with the highest ductility among the common commercially pure grades. | Use where formability, corrosion resistance, and low strength are the main priorities. | Suitable for applications that do not require the higher strength of alloyed grades. |
| Commercially Pure Titanium Grade 2 | Unalloyed titanium with a common balance of corrosion resistance, ductility, and strength. | Common general-purpose choice for chemical-processing, marine, heat-exchanger, and architectural components. | Usually easier to source globally than less frequently specified commercially pure grades. |
| Grade 5 Ti-6Al-4V | Alpha-beta titanium alloy containing approximately 6% aluminium and 4% vanadium by nominal composition. | Choose for high strength-to-weight requirements, aerospace components, tooling, and demanding mechanical parts. | Confirm the required material specification, heat-treatment condition, mechanical properties, and inspection level. |
| Grade 23 Ti-6Al-4V ELI | Extra-low-interstitial version of Ti-6Al-4V, normally selected where improved fracture toughness or biocompatibility requirements apply. | Specify the applicable medical or aerospace standard when the end use requires ELI material. | Grade 23 must not be substituted for Grade 5 without written engineering approval. |
| Grade 7 Titanium-Palladium | Commercially pure titanium with a small palladium addition for improved resistance in some reducing acid environments. | Consider for specialised chemical-processing service after checking the actual process chemistry. | Higher material cost and narrower availability make application-specific verification important. |
| 2. Diameter and Dimensional Tolerance |
| 10–18 mm diameter | ISO 286-2 h11 tolerance: 0 / −0.110 mm. | Maximum diameter: 18.000 mm; minimum diameter: 17.890 mm at the upper end of this size band. | Useful for machined parts when a controlled but economical bar tolerance is acceptable. |
| 18–30 mm diameter | ISO 286-2 h11 tolerance: 0 / −0.130 mm. | State the nominal diameter, tolerance class, measurement method, and measurement temperature in the purchase order. | Prevents different suppliers from interpreting “standard tolerance” differently. |
| 30–50 mm diameter | ISO 286-2 h11 tolerance: 0 / −0.160 mm. | Use a tighter tolerance only when machining allowance, fit, or material yield justifies the additional cost. | Tighter dimensional control can increase processing and inspection costs. |
| 50–80 mm diameter | ISO 286-2 h11 tolerance: 0 / −0.190 mm. | Confirm straightness and out-of-roundness separately; diameter tolerance alone does not control either property. | Large bars may meet diameter tolerance while still requiring straightening or additional machining. |
| 80–120 mm diameter | ISO 286-2 h11 tolerance: 0 / −0.220 mm. | Request a dimensional inspection report for critical or high-value orders. | Independent verification reduces disputes involving inspection location and measuring equipment. |
| 120–180 mm diameter | ISO 286-2 h11 tolerance: 0 / −0.250 mm. | Agree on permitted ovality, straightness, end condition, and bar length in addition to diameter. | These characteristics can affect cutting, turning, forging, and automated loading. |
| 180–250 mm diameter | ISO 286-2 h11 tolerance: 0 / −0.290 mm. | Confirm whether the product is supplied as a finished bar or as a billet intended for further processing. | Bars and billets can have different dimensional, surface, and inspection expectations. |
| 3. Surface Condition |
| Hot finished | Produced at elevated temperature; may retain an oxidised surface layer or alpha-case depending on processing and subsequent treatment. | Specify whether surface removal, descaling, or machining is required before acceptance. | Often economical for larger diameters, but it normally requires more finishing allowance than ground or polished bar. |
| Cold finished | Processed below the hot-working temperature to improve dimensional control and surface appearance. | Confirm the supplied condition, residual-stress requirements, and applicable mechanical-property limits. | Can reduce machining allowance but may have different residual-stress and straightness characteristics. |
| Peeled or turned | Surface is mechanically removed to eliminate or reduce scale and near-surface imperfections. | Specify minimum finished diameter, allowable tool marks, straightness, and end chamfer requirements. | Commonly selected when a clean, machinable surface is required without a fine-polished finish. |
| Ground | Abrasive finishing process that generally provides better surface uniformity and dimensional control than hot-finished material. | Define the required diameter tolerance and surface roughness target separately; a typical engineering target may be Ra ≤ 3.2 µm when agreed. | Surface roughness is not automatically established by the word “ground” and must be stated on the order. |
| Polished | Fine abrasive finishing used when appearance, cleanability, or a low-roughness surface is important. | Specify roughness, inspection method, allowable scratches, pits, stains, and protective packaging. | Polishing can improve appearance but does not replace requirements for grade, dimensions, or internal quality. |
| 4. Standards and Quality Documentation |
| Material specification | ASTM B348/B348M is a widely used specification for titanium and titanium-alloy bars and billets. | State the exact revision, grade, product form, heat-treatment condition, and supplementary requirements. | Standards with similar grade names can contain different chemical, mechanical, and testing requirements. |
| Dimensional tolerance standard | ISO 286-2 defines commonly used tolerance classes such as h11. | Write the complete tolerance designation, for example: “Ø40 mm, ISO 286-2 h11, 0/−0.160 mm.” | A complete designation is clearer than using an undefined term such as “commercial tolerance.” |
| Traceability | Heat number, chemical analysis, mechanical test results, and product identification should remain linked to the shipment. | Request a material test certificate with heat number, grade, size, condition, test results, and standard reference. | Traceability supports customs clearance, incoming inspection, and non-conformance investigation. |
| Inspection and testing | Potential requirements include chemical analysis, tensile testing, hardness, ultrasonic testing, surface inspection, and dimensional inspection. | List only the tests relevant to the application and define acceptance criteria before production. | Unspecified testing can create unexpected lead time, cost, or acceptance disputes. |
| 5. Recommended Purchase Order Format |
| Example description | Titanium round bar; Grade 5 Ti-6Al-4V; diameter 40 mm; ISO 286-2 h11, 0/−0.160 mm; peeled and turned surface; straightness and ovality to be agreed; cut length and quantity stated separately; material certificate required; applicable specification and revision stated; protective packaging required. |